MATERIAL QUALITY TEST AND ETA-APPROVAL.
|
|
|
|
|
|
|
|
|
|
|
|
|
In Europe,
all equipment installed in the drinking water supply is generally subject to material quality
test and final approval (ETA/GS/VA) before use. The test includes limited submission of heavy
metal particles as well as the necessary sustaining of pressure and tightness.
|
|
|
|
|
|
|
 |
|
|
|
|
|
|
|
|
|
TECHNICAL UNIVERSITY OF DENMARK, INSTITUTE OF APPLIED PHYSICS:
CALCIUM CRYSTAL AND LIME SCALE DEPOSIT PREVENTION TEST
|
|
|
|
|
|
|
|
|
|
 |
|
|
|
|
|
|
The Institute of applied physics at the Technical University of
Denmark is recognized for expertise in investigation and research of magnetic water conditioning
and in particular the ability to prevent lime scale. Investigation by the institute
has proved that turbulences in most products, rather than magnets, make changes of calcium
crystal structure. The dissolving of lime scale may give equal results by creating aggressive
CO2
from turbulent forces. Aqua Correct has a free and
smooth internal flow, which exclude the presence of turbulence. The function is pure magnetic
physical. The crystal change is clearly seen on the right after water evaporation
(75 x magnification).
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Upper photo, without
treated water:
60% limestone
deposits consisting of small hardening calcium crystals.
Lower photo, with t
reated water
(long term test):
After 14 days: Only
10% calcium crystal substances and still 90% prevention of lime scale deposits. The big
flakes (looking like snow) are the loose aragonite structure.
|
|
|
|
|
|
|
|
|
|
|
|
|
|
The conclusion of the
test results:
"the tests prove a powerful indication
of effective treatment conditioning".
BUILDING RESEARCH INSTITUTE: BACTERIAL
CONDITIONS IN WARM WATER SUPPLIES
|
|
|
|
|
|
|
|
|
|
Germs substance measurement (SBI report no. 235).
|
|
|
|
|
|
|
|
 |
|
|
|
|
|
The measuring results of
the diagram indicate the remarkable lower germ substance (two lower curves) after disconnection
of an electrolytic treatment in week 5 and the conversion to our physical
conditioning. The two upper curved with constant connected electrolytic
treatment contain germ substances, which are approximately 10 times higher and can not
be avoided, even by an effective magnetic water conditioner.
Conclusion:
Physical magnetic water treatment has an effect to
reduce germ substance in warm water systems.
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Update 1997:
The discovered decrease of germ substance
is a consequence of dissolving the lime scale deposits only.
|
|
|
|
|
|
|
|
|
|
 |
|
 |
|
 |
|
 |
|
|
|
|
|
|
|